Improvement of service life of turbine blade in wet region T-S-002
Mar. 12, 2012
T-S-002 / 766-90172
REASON FOR SUGGESTION:
A condensing turbine being operated in a wet steam region may have its blade surface erosion due to drain produced during long-term operation, leading to an accident of broken blade(s) in a worst case as well as reduction in efficiency.
DETAILS OF SUGGESTION:
Replace the blades (application limit of blade height : 200 mm) in a relatively high wet (<10%) stage with those so-called ceramic-ion plated which are Nitrided titanium (TiN)-top coat and chrome (Cr)-under coat. Thereby, higher erosion resistance and longer service life will be obtained.
技術情報
-
技術トピックス
- Super High Pressure Compressor
- Double Flow Integrally Geared Compressor (DF-IGC)
- MITSUBISHI Solution for LNG
- Value up (Compressors)
-
Value up (Mechanical Drive Steam Turbines)
- Improvement of service life of turbine blade in wet region T-S-002
- Improvement of drain erosion resistance for last stage blade T-E-009
- Repair of damaged rotor journal portion CT-S-025
- Application of diffusion treatment against solid particle erosion T-E-008
- Replacement of thrust bearing with improved type CT-S-023
- Thrust bearing with Ni-plating for ammonia plant CT-S-024
- Replacement with tilting pad bearing T-S-013
- Online washing system T-E-010
- Addition of partial stroke test device for Mechnical Trip Throttle Valve during operation T-S-006
- 製品カタログ
- 三菱重工技報